Table S1C2e FRLs deemed to be achieved by hot-rolled steel columns (including a fabricated column) exposed on not more than 3 sides
Specification 1 Fire-resistance of building elements
| Fire protection | Minimum thickness (mm) of principal material for FRLs | ||||
|---|---|---|---|---|---|
| 60/60/60 | 90/90/90 | 120/120/120 | 180/180/180 | 240/240/240 | |
| Concrete cast in-situ — load bearing | 25 | 30 | 40 | 55 | 75 |
| Concrete cast in-situ — non-load bearing unplastered | 25 | 30 | 40 | 50 | 75 |
| Concrete cast in-situ — non-load bearing plastered 13 mm | 25 | 25 | 30 | 40 | 50 |
| Gypsum cast in-situ | - | - | - | - | 50 |
| Gypsum — perlite or gypsum-vermiculite plaster—sprayed to contour | 20 | 25 | 35 | 50 | 55 |
| Gypsum — perlite or gypsum-vermiculite plaster—sprayed on metal lath | 20 | 20 | 25 | 35 | 45 |
Table Notes
For the purposes of this table, each element must meet the requirements of Specification 2.
Table for S1C2 Rating
Same wording in NCC 2022 Volume Two. See NCC 2022 Volume Two Table S1C2e.