Table · ABCB Housing Provisions 2022
Table 6.3.9a Minimum protective coatings for structural steel members
Part 6.3 Structural steel members
| Environment | Location | Minimum protective coating | ||
|---|---|---|---|---|
| Option 1 (hot dip galvanising) | Option 2 (duplex system). See Table 6.3.9c | Option 3 (paint). See Table 6.3.9b | ||
| Low (mild steel corrosion rate 1.3 to 25 μm/year | Typically remote inland areas or more than 1 km from sheltered bays | HDG75 | – | ACL2, ACC2, IZS1, PUR2A |
| Medium (mild steel corrosion rate 25 to 50 μm/year) | Typically more than 1 km from breaking surf or aggressive industrial areas or more than 50 m from sheltered bays | HDG225 | – | ACL3, ACC4, ACC5, IZS1, PUR3, PUR4 |
| High (mild steel corrosion rate 50 to 80 μm/year) | Typically more than 200 m from breaking surf or aggressive industrial areas or within 50 m from sheltered bays | HDG450 | HDG150 (5 years) 4D (10-15 years) or HDG300 (10 years) 2D (5-10 years) | ACC6, IZS3, PUR5 |
| Very High (mild steel corrosion rate 80 to 200 μm/year) | Typically extends from 100 m inland from breaking surf to 200 m inland from breaking surf, or within 200 m of aggressive industrial areas and within 100 m of breaking surf. | HDG900 | HDG300 (5 years) 5D (10-15 years) or HDG600 (10 years) 4D (5-10 years) | ACC6 (C5-M only), PUR5 |
Table Notes
Hot dip galvanising and duplex systems must be in accordance with AS 2312.2. Paint systems must be in accordance with AS 2312.1.
Table for 6.3.9 Corrosion protection
Same wording in ABCB Housing Provisions 2025. See ABCB Housing Provisions 2025 Table 6.3.9a.