Table 6.3.9a Minimum protective coatings for structural steel members

Part 6.3 Structural steel members

Open Table 6.3.9a on NCC Online ↗
EnvironmentLocationMinimum protective coating
Option 1 (hot dip galvanising)Option 2 (duplex system). See Table 6.3.9cOption 3 (paint). See Table 6.3.9b
Low (mild steel corrosion rate 1.3 to 25 μm/yearTypically remote inland areas or more than 1 km from sheltered baysHDG75–ACL2, ACC2, IZS1, PUR2A
Medium (mild steel corrosion rate 25 to 50 μm/year)Typically more than 1 km from breaking surf or aggressive industrial areas or more than 50 m from sheltered baysHDG225–ACL3, ACC4, ACC5, IZS1, PUR3, PUR4
High (mild steel corrosion rate 50 to 80 μm/year)Typically more than 200 m from breaking surf or aggressive industrial areas or within 50 m from sheltered baysHDG450HDG150 (5 years) 4D (10-15 years) or HDG300 (10 years) 2D (5-10 years)ACC6, IZS3, PUR5
Very High (mild steel corrosion rate 80 to 200 μm/year)Typically extends from 100 m inland from breaking surf to 200 m inland from breaking surf, or within 200 m of aggressive industrial areas and within 100 m of breaking surf.HDG900HDG300 (5 years) 5D (10-15 years) or HDG600 (10 years) 4D (5-10 years)ACC6 (C5-M only), PUR5

Table Notes

Hot dip galvanising and duplex systems must be in accordance with AS 2312.2. Paint systems must be in accordance with AS 2312.1.

Table for 6.3.9 Corrosion protection

Same wording in ABCB Housing Provisions 2022. See ABCB Housing Provisions 2022 Table 6.3.9a.